Skip to main content
. 2019 Aug 29;10:1789–1801. doi: 10.3762/bjnano.10.174

Figure 1.

Figure 1

Variation of the Z-average mean diameters, Dz, of SLNs (A, B) and NLCs (C, D) produced in the absence of antioxidants and NLC loaded with TOC (E, F) evaluated at 1 (light grey) and 90 (grey) days after nanoparticle production. In the case of SLN T10, SLN C10 and SLN P10, mean diameters were not measurable by PCS 90 days after production.