Skip to main content
. 2019 Aug 8;12(16):2529. doi: 10.3390/ma12162529

Figure 1.

Figure 1

Figure 1

X-ray diffraction patterns (XRD) of different zirconia ceramics for extreme sintering temperatures: (a) 1450 °C, (b) 1560 °C, and (c) detail of 2 theta between 34–37° and 45–70°, the region with the greatest variation of ZrO2-cubic and ZrO2-tetragonal perceptual.