Table 2.

Differential Scanning Calorimetry (DSC) analysis on the different material formulations. Statistical differences are defined by p-value > 0.05 (*) in each EVA subgroup.

Polymer Formulation Melting Point (°C) Crystallinity (%)
EVA18 83.1 ± 2.2 23.4 ± 4.1 (*)
EVA18 20% BaTiO3 85.1 ± 0.3 33.8 ± 1.9 (*)
EVA18 20% ZnO 85.5 ± 0.5 29.7 ± 4.5
EVA25 77.3 ± 1.4 (*) 24.8 ± 0.4 (*)
EVA25 20% BaTiO3 78.9 ± 5.3 28.9 ± 5.7
EVA25 20%ZnO 85.2 ± 0.7 (*) 31.7 ± 0.8 (*)
EVA40 46.7 ± 0.3 9.8 ± 0.5
EVA40 20% BaTiO3 46.7 ± 0.8 10.2 ± 0.4
EVA40 20% ZnO 46.1 ± 0.9 8.8 ± 3.2