Skip to main content
. 2019 Mar 30;141(16):6537–6544. doi: 10.1021/jacs.8b12284

Figure 7.

Figure 7

Depth profiling analysis of graphene-covered Pt nanoparticles/layers of various thickness on FAD55 in 0.1 M H2SO4 electrolyte, performed at 1.85 VRHE after a dwell period of at least 10 min. For fitting procedure, see section S2 in the ESI. The fraction of oxidic Pt was taken as the combined Pt2+ and Pt4+ contribution to the fitted spectra.