Figure 3.

Figure 3.

Polarized light photomicrographs for the PS/PO oil blends under 60 MPa high-pressure microfluidization (HPM) treatment. A, Treated once and crystallized 0 hour, 4 hours, 1 day, and 5 days. B, Treated twice and crystallized 0 hour, 4 hours, 1 day, and 5 days, respectively. Magnification 500 × 19.