Skip to main content
. Author manuscript; available in PMC: 2019 Sep 11.
Published in final edited form as: Sci Total Environ. 2017 Sep 20;613-614:714–723. doi: 10.1016/j.scitotenv.2017.09.050

Figure 4:

Figure 4:

Release of cerium from MCA-coated boards that have undergone 1260 h of UV degradation before application of surface coatings. Data were collected in triplicate and have been normalized by the total area wiped during a sampling event. The data at Time zero correspond with the first wipe event after application of surface coatings and dry time of at least 48 h.