Skip to main content
. 2019 Apr 11;14(3):309–317. doi: 10.1016/j.jds.2018.11.008

Figure 8.

Figure 8

The fractured surface of a sample with fiber reinforcement (1000× magnification). The outer layer of glass fiber separated from the resin (⇦) and left a mark on the resin matrix, indicating the excellent impregnation between the fiber and matrix.