Figure 1.

Figure 1.

Stress relaxation of A. subfuscus glue. Samples were rapidly stretched to a strain of 2, and then held at constant strain. Three trials from separate glue samples are shown superimposed. The initial stress at a strain of 2 was 42 ± 8.5 kPa.