Skip to main content
. 2019 Sep 16;9:13324. doi: 10.1038/s41598-019-49639-3

Figure 10.

Figure 10

Dielectric properties of the dielectric thick films prepared with (A2) (66 vol% BST), (B2) (50 vol% BST) and (C2) (33 vol% BST). Left side: permittivity εr, right side: loss tangent tan δ.