Figure 6.

Figure 6

Overview of the printed electrodes after temperature treatment of 120 °C for 1 h. Upper row (a–c) displays the top electrode and lower row (d–f) the bottom electrode. Optical microscope images (a,d), topography images (b,e) and 2D-profiles (c,f).