Table 3.

Compressive strengths of high-early-strength cement with different dispersed processes and unprocessed short carbon fibers. (Unit: MPa).

Benchmark High Temperature Acid Water Alkali
46.5 54.9 51.9 47.6 48.6
43.5 53.0 49.0 47.5 49.4
43.7 53.2 48.3 46.7 46.0
42.8 49.2 48.4 48.7 45.9
45.7 51.7 50.6 47.1 45.7
45.4 45.6 51.8 47.0 46.7