Skip to main content
. 2019 Aug 1;52(15):6005–6017. doi: 10.1021/acs.macromol.9b01083

Figure 7.

Figure 7

LCP particle morphology of extruded strands after heating to the processing temperature for 1 min. From left to right: 10 wt % LCP-A in PLLA, 10 wt % LCP-B in PLLA, particle size distribution of 10 wt % LCP-B in PLLA. Note, the PLLA matrix was dissolved in a 1:3 mixture of acetone/dichloromethane prior to capturing the LCP particle image.