Characterization of PC10A/DOX/HAuNS nanogels and PC10A/DOX/HAuNS hydrogels. a TEM image and high resolution TEM image (insert) of HAuNS; b the different orientate lattice of HAuNS; TEM image of HAuNS/DOX nanoparticles (c) and PC10A/DOX/HAuNS nanoparticles (d); e zeta potentials of HAuNS, DOX/HAuNS nanoparticles, and PC10A/DOX/HAuNS nanoparticles; f UV–vis absorbance spectra of HAuNS solution, DOX solution, and DOX/HAuNS solution; g photographs of PC10A hydrogel, PC10A/DOX hydrogel, PC10A/HAuNS hydrogel, and PC10A/DOX/HAuNS hydrogel (PC10A: 3% w/w, DOX: 0.8 mg mL−1, HAuNS: 20 μg mL−1); h SEM image and the high resolution SEM (insert) of the PC10A/DOX/HAuNS hydrogel