Biocompatibility of PC10A nanogels and hemolysis ration of PC10A hydrogel. The cell viability of HepG2 cells incubated with different concentrations of PC10A nanogels (a) and HAuNS (b); c hemolysis ration of PC10A hydrogel and PC10A/HAuNS hydrogel incubated with RBC for a series of time points (2, 4, and 8 h); dg 3D cell culture of HepG2 cells in PC10A hydrogel (3% w/w) and PC10A/HAuNS hydrogel (PC10A: 3% w/w; HAuNS: 20 μg mL−1) for 24 h and 48 h