Cross‐sectional SEM images of the PCSF host after plating a1–3) 1 mAh cm−2, b1–3) 3 mAh cm−2, c1–3) 8 mAh cm−2, and d1–3) 10 mAh cm−2. e) Schematic illustration of the Li plating in the PCSF host at different states.