Figure 8.

Figure 8.

Longitudinal bone volume as measured with μCT. * p=0.011 between both BMP groups and the Gel Only material control group. B) Failure strength and C) Stiffness of regenerated bone tissue at the 12 week endpoint. * p<0.001 between all treatment groups and the contralateral control.