Published in final edited form as: ACS Appl Bio Mater. 2018 Dec 11;2(1):81–92. doi: 10.1021/acsabm.8b00390

Figure 1.

Figure 1.

Hydrolysis of PEG-norbornene hydrogel scaffolds without hMSCs. (a) Bulk rheological measurements of the elastic moduli, G′, as a function of time throughout degradation. (b) Normalized elastic moduli, G/G0, as a function of time. This data is fit to eq 2, resulting in a hydrolysis kinetic constant, kh = 7.5 × 10−3 ± 7.1 × 10−4 h−1.