Published in final edited form as: Biomaterials. 2019 Aug 13;223:119430. doi: 10.1016/j.biomaterials.2019.119430

Table 1:

Hydrogel formulations used in this study. Concentrations are reported in mM. Storage (G’) and loss (G”) moduli were measured at 1 rad s−1. Formulations used in cellular experiments are highlighted.

Ela PBA 50 PBA 100 PBA 200 Glu 100 Glu 200 Glu3 00 Glu 400 Man 100 Man 200 Man 300 Man 400
PBA-Ac 0 50 100 200 200 200 200 200 200 200 200 200
Glu-Ac 0 0 0 0 100 200 300 400 0 0 0 0
Man-Ac 0 0 0 0 0 0 0 0 100 200 300 400
PEG-MeO Ac 700 650 700 500 400 300 200 100 400 300 200 100
G’(kPa) 13.8 12.1 11.5 21.1 16.8 14.8 12.8 9.3 13.8 11.6 9.8 6.5
G“ (kPa) 0.0 0.0 0.3 2.4 1.7 1.9 1.7 1.5 1.1 1.0 0.7 0.6