Skip to main content
. 2019 Sep 4;12(18):2853. doi: 10.3390/ma12182853

Table 2.

Optimized parameters related to consolidation deformation at different temperatures.

260 °C 270 °C 280 °C 300 °C Units
D1 2.274 × 10−2 6.814 × 10−2 2.177× 10−2 8.793 × 10−2 [J mm−2]
D2 4.113 × 10−1 5.870× 10−1 3.607× 10−1 6.889× 10−1 [J mm−2]
D3 2.478 1.080 1.279 1.466 [J mm−2]
D4 5.386 3.434 × 10-1 1.974 -3.411 [J mm−2]
D5 4.170 1.383 −9.312 × 10−1 6.299 × 10−1 [J mm−2]
γ1 7.293 1.043 5.236 × 10−1 8.024 × 10−1 -
γ2 4.499 × 10−1 5.754 × 10−1 9.420 × 10−2 4.443 × 10−1 -
τ1 35.87 8.473 × 10−1 5.787 × 10−2 3.638 × 10−1 [s]
τ2 20.37 6.724 × 10−1 3.262 × 10−1 3.881 × 10−1 [s]