Table 2.
Swell Ratio of Different Hep-HA Hydrogels
| sample | soft Hep- HA |
stiff Hep-HA |
|---|---|---|
| polymer concentration | 2 wt % | 4 wt % |
| before swelling storage modulus (G’ = Pa) | 573 ± 46a | 1762 ± 197a |
| after swelling storage modulus (G’ = Pa) | 333 ± 60a | 1176 ± 137a |
| swelling ratio (Ws/Wd) | 47.9 ± 7.3 | 29.4 ± 3.2 |
p < 0.05 between soft and stiff Hep-HA hydrogels.