Skip to main content
. 2019 Oct 1;9:14040. doi: 10.1038/s41598-019-50247-4

Figure 2.

Figure 2

Mechanical integrity of the 200 nm ITO film embedded into a PDMS substrate: (a) outer bending and (b) inner bending test compared to 200 nm of ITO film deposited on to PDMS. SEM images of Flexible ITO embedded in PDMS (c) and deposited on PDMS.