Skip to main content
. 2019 Sep 12;11(9):1492. doi: 10.3390/polym11091492

Figure 3.

Figure 3

IR spectra of the electrospun PEO fibers (a), the electrospun PLA fibers (b and e), the as-spun PEO/PLA blend fibers (c), the blend fibers upon the removal of PEO (d), the PLA-PGS composite membrane (f), the composite membrane upon the removal of PLA (g), and the PGS solid sheet (h). Note that the all PGS samples were cured under 120 °C for 48 h.