Skip to main content
. 2019 Aug 31;11(9):1431. doi: 10.3390/polym11091431

Table 6.

Results of linear dimension changes, geometrical volume changes and mass loss of obtained foams.

Test M0 M30 M40 M50 M60
Δl (%) −2.4 ± 0.1 +0.9 ± 0.1 +0.9 ± 0.1 +0.7± 0.1 +0.8 ± 0.1
ΔV (%) +2.8 ± 0.1 +1.0 ± 0.1 +0.5 ± 0.1 +1.0± 0.1 +1.0 ± 0.1
Δm (%) 3.1 ± 0.1 1.0 ± 0.1 0.2 ± 0.0 0.5 ± 0.0 0.1 ± 0.0