Skip to main content
. 2019 Sep 18;11(9):1516. doi: 10.3390/polym11091516

Figure 16.

Figure 16

SEM micrographs of (a) pure POM, (b) pure PLA, and their blends with (c) 10 wt %, (d) 20 wt %, (e) 30 wt %, (f) 40 wt % and (g) 50 wt % PLA after enzymatic degradation.