Skip to main content
. 2019 Sep 12;11(9):1489. doi: 10.3390/polym11091489

Figure 4.

Figure 4

Weight loss (%) versus degradation time for the samples T1, T2, and HDPE at (a) 30 °C and (b) 50 °C. T1 = Mater Bi®-based pipes, and T2 = Bio-Flex®-based pipes.