Skip to main content
. 2019 Sep 16;11(9):1511. doi: 10.3390/polym11091511

Table 1.

Composite solution and nanofiber performance.

Samples Diameter (nm) Viscosity (Pa·S) Conductivity (mS/cm)
Ker.0%/PA6 293 ± 70 2.48 3.18
Ker.30%/PA6′ 229 ± 74 1.95 4.15
Ker.30%/PA6 192 ± 65 1.09 4.45
Ag.1%-Ker.30%/PA6 183 ± 40 0.94 4.67
Ag.10%-Ker.30%/PA6 168 ± 60 0.85 6.83
Ker.50%/PA6 174 ± 49 0.78 5.26
Ker.70%/PA6 155 ± 50 0.70 6.53