Skip to main content
. 2019 Sep 18;11(9):1517. doi: 10.3390/polym11091517

Figure 6.

Figure 6

Figure 6

SEM micrographs of electrospun structures obtained from HA/PEO blend solutions. (a) HA 243 kDa, PEO 300 kDa. (b) HA 370 kDa, PEO 300 kDa. (c) HA 600 kDa, PEO 300 kDa. (d) HA 243 kDa, PEO 600 kDa. (e) HA 370 kDa, PEO 600 kDa. (f) HA 600 kDa, PEO 600 kDa.