Skip to main content
. 2019 Jul 30;6(3):65. doi: 10.3390/bioengineering6030065

Figure 6.

Figure 6

Wound dressings cross-linked with CaCl2 (50 mM). Note the relatively large shrinkage of the samples containing alginate. The target dimensions of the 3D printed structures were 20 mm × 40 mm.