Table 7.
Author | Test | Aging | Storage | Highest Value/Lowest Value (MPa) |
---|---|---|---|---|
Saulo Pamato | Microshear bond strength | ______________ | _____________ | Adper Single Bond 2: 16<break/>U 200: 11.190 |
Pekperdahci | Microshear bond strength | Water 5 °C/55 °C for 10,000 cycles | Distilled water at 37 °C for two days | ARC Single Bond 2: 370.07 Relyx Unicem/Adper Prompt 77.06 |
Chávez | Microshear bond strength | _____________ | Distilled water and kept at a constant temperature of 37 °C | Relyx ARC Single Bond 2: 15.52 Set PP 3.17 |
Ozturk | Microshear bond strength | Thermocycled between 5 °C and 55 °C in Deionized water for 5000 cycles. | Distilled water for 24 h at 37 °C | Variolink Venner/Heliobond: 24.76 (enamel) RelyX Veneer/Adper Scottchbond: 5.42 (dentin) |
Lorenzoni | Microshear bond strength | ______________ | ________________ | Adper Single Bond 2/Duo Link: 14.5 All Bondl/Duo Link: 6.16 |
Aguiar | Microtensile bond strength | Mechanical load cycling, submitted to 50,000 cycles | Artificial saliva for 1 day | Relyx Unicem: 21.3 Clearfil Esthetic Cement/Clearfil DC Bond: 13.3 |
Vaz | Microtensile bond strength | ______________ | 37 °C and 100% relative humidity | Relyx ARC/Adper Single Bond 2: 40.8 C&B Cement/All-Bond 2: 19.5 |
Bacchi | Microtensile bond strength | Pulpal pressure for 3 months | 20 cm distilled water | Relyx ARC/Adper single bond 2: 25 U200: 8 |
Alexandre | Microtensile bond strength | Pulpal pressure for 24 h | Distilled water | Clearfil SE Bond/Panavia F: 38.0 Panavia 21/Panavia F2.0: 7.8 |
Roperto | Microtensile bond strength | _______________ | Water for 24 h at 37 °C | Primer and Bond NT/Calibra: 17.68 Smart Cem: 6.48 |
Skupien | Microtensile bond strength | Distilled water at 37 °C for 24 h | Adper Scotchbond/Relyx ARC: 20.29 U100: 9.69 |