Fig 1. Schematic of aluminum ZMW fabrication.

Fig 1

The starting material is a glass microscope coverslip. Steps in fabrication and listed and explained in the main text. Black boxes represent expanded insets. Tg is the glass transition temperature of the polystyrene micro-spheres.