Open circuit potential for the InN/InGaN reference electrode. (A) OCP as a function of time for the 0.8-ML-InN/35-nm-In0.45Ga0.55N electrode and Ag/AgCl reference electrode successively immersed for 150 seconds in 0.001, 0.01, 0.1 and 1 M KCl aqueous solutions. (B) Long-time OCP measurement for the same sample over 12 hours in 0.1 M KCl aqueous solution. (C,D) OCP as a function of time for the 0.8-ML-InN/35-nm-In0.45Ga0.55N electrode and Ag/AgCl reference electrode immersed alternately for 150 seconds (C) in water and pH 8.5 KOH aqueous solutions and (D) in 0.1 and 1 M KCl aqueous solutions at 50 °C.