Skip to main content
. 2019 Oct 11;9:14671. doi: 10.1038/s41598-019-51123-x

Figure 2.

Figure 2

Immersion test using artificial intestinal juice. Macroscopic view of the developed Mg alloy staples at zero, one, four, eight, and 12 weeks after immersion (above) and Mg alloy staples removed after immersion (lower). The surfaces of the staples were covered with a layer of white corrosion product.