Skip to main content
. 2019 Oct 8;14:8149–8159. doi: 10.2147/IJN.S214646

Figure 6.

Figure 6

AFM images of (A) PE, (B) PE/WG and (C) PE/WG/TiO2. Sample with size of 1 cm * 1 cm was cut and scanned in 20 * 20 µm size with 256 * 256 pixels under normal atmosphere in Nanowizard, JPK instruments.