Room temperature sodium-sulfur battery test. a Cycling performance of NiS2@NPCTs/S (red) and NPCTs/S (black) at a current density of 1 A g−1. b The corresponding charge/discharge profiles of NiS2@NPCTs/S at different cycles. c Rate capability at 0.1, 0.2, 0.5, 1, 2, and 5 A g−1 for NiS2@NPCTs/S (red) and NPCTs/S (blue). d The corresponding charge/discharge profiles of NiS2@NPCTs/S at different current densities