Skip to main content
. 2019 Oct 4;19(19):4296. doi: 10.3390/s19194296

Table 2.

Magnetoelastic characterization values obtained from the resonance/anti-resonance frequency measurements for strips with R = 6 equal or close value.

L (mm) w (mm) R = L/w Emin(GPa) ES(GPa) ΔE (%) Hk* (A/m) kmax Q (kmax) ΔH (A/m)
30 5 6 154.3 163.6 5.7 619.8 0.23 33.4 682.9
20 3.33 6.1 152.8 163.5 6.6 675.7 0.23 28.9 583.9
15 2.5 6 154.7 164.7 6.1 776.2 0.19 31.2 708.4
10 1.66 5.9 154.6 164.2 5.9 1005.2 0.14 32.5 819.3