In vitro and in vivo bioactivity of bioactive glass. (a) Scheme of apatite formation on the surface of bioactive glass [114]. (b–c) SEM images of the layer-structured hydroxyapatite microspheres converted from 2Na2O–2CaO–6B2O3 bioactive glass in vitro [69]. (d) BSE-SEM images and elemental mappings for Ti (blue), Ca (red), Si (green) of sol–gel bioactive glass coated porous Ti after 4 weeks of implantation in a rabbit tibia defect [121].