Table 2.

The material properties for LV (#2) and BV (#6) models with highest heterogeneous regional contraction (Tmax). For the LV model (model #2 in Table 1), Tmax values at regions 1–16 were 36.2, 345.3, 175.5, 108.3, 71.7, 90.4, 41, 177.1, 680.4, 46.1, 60.9, 55.1, 23.6, 426.9, 37.2, and 31.5 kPa. For the BV mode (model #6 in Table 1), Tmax values at regions 1–16 were 113.0, 113.0, 400.0, 400.0, 400.0, 400.0, 113.0, 113.0, 113.0, 113.0, 280.0, 113.0, 113.0, 113.0, 113.0, and 113.0 kPa. The results from a previous report are provided for comparison. For models 2 and 3, the regional contractions were calculated in a way similar to model 1.

Parameters
Model a, MPa b af, MPa bf as, MPa bs afs, MPa bfs Tmax MPa
1 5.913 × 10−4 7.899 1.949 × 10−3 15.157 2.707 × 10−4 13.142 1.590 × 10−4 3.235 0.075
2 5.913 × 10−4 7.899 1.949 × 10−3 15.157 2.707 × 10−4 13.142 1.590 × 10−4 3.235 Caption
3 5.913 × 10−4 7.899 1.949 × 10−3 15.157 2.707 × 10−4 13.142 1.590 × 10−4 3.235 Caption
4 5.913 × 10−4 7.899 1.949 × 10−3 15.157 2.707 × 10−4 13.142 1.590 × 10−4 3.235 Caption
5 [13] 1.704 × 10−4 5.517 5.618 × 10−4 10.586 7.803 × 10−5 9.179 4.584 × 10−5 2.259 0.113
6 1.704 × 10−4 5.517 5.618 × 10−4 10.586 7.803 × 10−5 9.179 4.584 × 10−5 2.259 Caption
Dabiri et al. [6] 6.832 × 10−4 7.541 2.252 × 10−3 14.471 3.127 × 10−4 12.548 1.837 × 10−4 3.088 0.086