Skip to main content
. 2019 Oct 15;12(20):3352. doi: 10.3390/ma12203352

Figure 5.

Figure 5

(a) Load-deflection curves of F1FU specimens during repeated loading test including static test results after one million cycles. (b) A detailed view of the first initial deflection 2.5 mm.