Skip to main content
. 2019 Oct 15;12(20):3352. doi: 10.3390/ma12203352

Figure 7.

Figure 7

Crack patterns at failure during monotonic loading: (a) S1FU specimen (no fatigue loading) and (b) F1FU specimen.