Skip to main content
. 2019 Oct 17;12(20):3402. doi: 10.3390/ma12203402

Figure 13.

Figure 13

Micro-Vickers hardness values obtained at individual foils on edge and dome regions (a) for a bulged sample at RT and (b) for a bulged sample at 300 °C.