Skip to main content
. 2019 Oct 15;12(20):3370. doi: 10.3390/ma12203370

Figure 6.

Figure 6

Cross sections from sample 3D-3f-H0-P1.7 before (a) and after the (b) reciprocal wear test, showing surface morphology and coating layer cross sections.