. 2019 Oct 15;12(20):3370. doi: 10.3390/ma12203370

Figure 7.

Figure 7

Cross sections from sample 3D-3f-H3-P3.4-C before (a) and after the (b) reciprocal wear test, showing surface morphology and coating layer cross sections.