Figure 4.

Figure 4

Long-duration lcPET hydrolysis reaction (1.2 cm2 mL−1) with 1 µM TfCut2 in the presence (green diamonds) or absence (blue diamonds) of 30 ppm C12-N(CH3)3+ at 65 °C. Weight loss of the lcPET films was calculated from the amount of released compound at each reaction time. The error bars denote the standard deviation calculated from three different experiments.