Preparations of the CNT–CF wet-laid composites.

Sample Code CNT 0 wt % CNT 1 wt % CNT 5 wt % CNT 10 wt % CNT 20 wt %
PA fiber 0 wt % P1-C0 P1-C1 P1-C5 P1-C10 P1-C20
PA fiber 50 wt % P2-C0 P2-C1 P2-C5 P2-C10 P2-C20
PA fiber 100 wt % P3-C0 P3-C1 P3-C5 P3-C10 P3-C20

* PA6 and CNT: wt % with respect to carbon fiber. PA6 film for film stacking process: 58g/m2, 0.06 mm.