Skip to main content
. 2019 Oct 21;4(19):18257–18267. doi: 10.1021/acsomega.9b02271

Figure 2.

Figure 2

Appearance of the cuboid foams before (left) and after 16 h of swelling in water (right): (a) WG, (b) WG/CNF, (c) WG/GEN, and (d) WG/CNF/GEN.