Concentration of elements (wt. %) measured with EDS spectroscopy on polymer PS doped with 10%–40% GNP or samples doped with 10% of GNP treated with a laser fluence of 8–40 mJ·cm−2. View field of 30 × 30 μm2.

Laser Modified Samples (W(GNP) = 10%) Non-Modified Samples
E (mJ cm−2) C (wt. %) O (wt. %) GNP (wt. %) C (wt. %) O (wt. %)
8 89.03 ± 0.08 10.97 ± 0.08 10 99.29 ± 0.03 0.71 ± 0.03
16 92.89 ± 0.07 7.11 ± 0.07 20 99.30 ± 0.04 0.70 ± 0.04
20 90.98 ± 0.07 9.02 ± 0.07 30 99.28 ± 0.07 0.72 ± 0.07
40 91.32 ± 0.04 8.68 ± 0.04 40 99.34 ± 0.04 0.66 ± 0.04