Skip to main content
. 2019 Nov 4;12(21):3627. doi: 10.3390/ma12213627

Figure 9.

Figure 9

Samples of alloy WE43 and tissues of the implantation area six weeks after surgery: complete degradation of the sample in the initial state of the alloy, a small amount of biodegradation products of the alloy was found only in the skin scab (a); capsule formation around the sample in the UFG state of the alloy and gas accumulation in its cavity (b); the results of histological examination of mouse tissues (HE staining) in the area of contact with the samples in the initial (c,d) and the MAD-processed (e) states of the alloy.