Skip to main content
. 2019 Oct 26;12(21):3520. doi: 10.3390/ma12213520

Figure 7.

Figure 7

Microstructures of the TC4 alloy deformed at different strain rates (T = 860 °C). (a) 5 × 10−4 s−1; (b) 10−3 s−1; (c) 5 × 10−3 s−1; (d) 5 × 10−2 s−1.