Skip to main content
. 2019 Oct 26;12(21):3520. doi: 10.3390/ma12213520

Figure 12.

Figure 12

TEM microstructures of the Ti–6Al–4V alloy at 890 °C (ε = 0.6). (a) 5 × 104 s−1 and (b) 0.05 s−1.