Activation energy Q (±7.7) during superplastic deformation of the TC4 alloy.

T, °C 800 830 860 890
Strain Rate ε˙, s−1
5 × 10−4 328.88 400.89 429.08 389.35
5 × 10−3 344.52 418.80 449.33 407.99
10−3 338.96 412.09 442.14 401.44
5 × 10−2 427.54 519.22 546.90 505.87